MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Shin-Etsu Silicones KEP-12 Silicone additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: KEP12 is an additive which can be used in most of the silicone products to improve heat stability.

Product Features:

  • Improve thermal stability and compression set.
  • Excellent dispersion.

Information Provided by Shin-Etsu Silicones of America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.66 g/cc1.66 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5656
Tensile Strength at Break 10.7 MPa1550 psi
 
Descriptive Properties
Cure AgentDMBPH
 DMPH
Cure TypePost Cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shin-Etsu Silicones KE-347T Silicone, RTV Coating
Shin-Etsu Silicones KE-441 Silicone, RTV
Shin-Etsu Silicones KE-5551U High Strength Silicone Elastomer
Shin-Etsu Silicones KE-5560U Low Temperature Silicone Elastomer
Shin-Etsu Silicones KE-9610U Silicone Elastomer

PSHIN249 / 177760

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.