MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

The NanoSteel® Company SHS 7174 TWAS Steel Alloy, Cored Wire  (discontinued **)
Categories: Metal; Ferrous Metal; Alloy Steel; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Coating Description: SHS 7174 TWAS is an iron based steel alloy with a nanoscale microstructure that features good resistance to wear, abrasion, impact, corrosion, high temperature erosion and sulfidation attack.

    Key Performance Characteristics
  • Excellent corrosion and wear resistance
  • High impact resistance
  • Especially resistant to elevated temperature sulfidation attack
  • Cost-effective option for elevated temperature erosion/corrosion protection of heat exchange tubes in coal fired boilers

Application Process: Twin Wire Arc Spraying (TWAS)

Information Provided by The NanoSteel Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.42 g/cc0.268 lb/in³Coating Property
Porosity <= 5.0 %<= 5.0 %Coating Property
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 965 - 1065965 - 1065kg/mm2; HV300
Adhesive Bond Strength 3.45 - 48.3 MPa
@Thickness 0.508 mm
500 - 7000 psi
@Thickness 0.0200 in
1018 steel; ASTM C633-01
 
Component Elements PropertiesMetricEnglishComments
Boron, B <= 5.0 %<= 5.0 %
Carbon, C <= 2.0 %<= 2.0 %
Chromium, Cr <= 30 %<= 30 %
Iron, Fe >= 45 %>= 45 %
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo <= 10 %<= 10 %
Silicon, Si <= 2.0 %<= 2.0 %
Tungsten, W <= 4.0 %<= 4.0 %
 
Descriptive Properties
Deposition Efficiency (%)80Coating Property
Impact ResistanceNo delamination/cracking at 480 in-lbsDrop Impact Testing
Wear Resistance Mass Loss (g)0.212000 cycles; ASTM G65-04 Procedure B

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NNANO106 / 106800

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.