MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ovako S235JR EN10025-2 (ref) Steel, +AR
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Soft structural steel easy to weld and bend.

Information provided by Ovako

Key Words: SS 1312, S235JR, 1.0038, Fe 360 BFN, RSt37-2, 40 B
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 340 - 490 MPa
@Thickness 150.1 - 200 mm
All formats
 350 - 500 MPa
@Thickness 100.1 - 150 mm
All formats
 360 - 510 MPa
@Thickness <=16.0 mm
All formats
 360 - 510 MPa
@Thickness 16.1 - 40.0 mm
All formats
 360 - 510 MPa
@Thickness 40.1 - 63.0 mm
All formats
 360 - 510 MPa
@Thickness 63.1 - 100 mm
All formats
Tensile Strength, Yield >= 185 MPa
@Thickness 150.1 - 200 mm
Reh, All formats
 >= 195 MPa
@Thickness 100.1 - 150 mm
Reh, All formats
 >= 215 MPa
@Thickness 40.1 - 63.0 mm
Reh, All formats
 >= 215 MPa
@Thickness 63.1 - 100 mm
Reh, All formats
 >= 225 MPa
@Thickness 16.1 - 40.0 mm
Reh, All formats
 >= 235 MPa
@Thickness <=16.0 mm
Reh, All formats
Elongation at Break 21 %
@Thickness 150.1 - 200 mm
All formats
 22 %
@Thickness 100.1 - 150 mm
All formats
 24 %
@Thickness 63.1 - 100 mm
All formats
 25 %
@Thickness 40.1 - 63.0 mm
All formats
 26 %
@Thickness <=16.0 mm
All formats
 26 %
@Thickness 16.1 - 40.0 mm
All formats
Modulus of Elasticity 210 GPa
Poissons Ratio 0.30
Shear Modulus 80.0 GPa
Impact Test 27.0 J
@Thickness <=16.0 mm,
Temperature 20.0 °C
All formats
 27.0 J
@Thickness 16.1 - 40.0 mm,
Temperature 20.0 °C
All formats
 27.0 J
@Thickness 40.1 - 63.0 mm,
Temperature 20.0 °C
All formats
 27.0 J
@Thickness 63.1 - 100 mm,
Temperature 20.0 °C
All formats
 27.0 J
@Thickness 100.1 - 150 mm,
Temperature 20.0 °C
All formats
 27.0 J
@Thickness 150.1 - 200 mm,
Temperature 20.0 °C
All formats
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 40.0 - 45.0 W/m-KAmbient temperature
Transformation Temperature 485 °CMS
 725 °CAC1
 863 °CAC3
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.17 %
Copper, Cu <= 0.55 %
Iron, Fe >= 97.8 %As Balance
Manganese, Mn <= 1.4 %
Nitrogen, N <= 0.012 %
Phosphorus, P <= 0.035 %
Sulfur, S <= 0.035 %
 
Descriptive Properties
WeldabilityCEV 0.35max
 Pcm 0.25max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ovako S235JR SS 14 13 12:1987 (ref) Steel, +AR
EN S235JR High Manganese, Structural, Hot Rolled, Base Steel, t < 16 mm
American Yellow Birch Wood
ASTM A284 Steel, grade C
EN S235JR Structural, Hot Rolled, Base Steel, 16 mm < t < 25 mm

NOVAKO410 / 234709

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.