Russian Al-Li Alloy (Russian Federation Patent No. 1584414) used in aerospace cryogenic fuel tanks. Has low density and exhibits high strength, high elasticity, and high fatigue durability at both elevated (up to150°C) and cryogenic temperatures. |
Russian Aluminum-Lithium 1460 Alloy, Al-Li Alloys, Aluminium Alloy; Al1460 |