MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Scotchcal™ 3632-76 Translucent Film
Categories: Polymer; Film

Material Notes: 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that increases durability and cleanability (Film 3632GPS is the same as 3M Scotchcal Translucent Series 3630 with the addition of GPS); Clear pressure-sensitive adhesive; Synthetic layflat liner that is not affected by water or humidity; Designed especially for electronic cutting; Thermoformable; For flat surfaces; 22 crisp clear colors, many with simulated PANTONE® color references

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milwithout adhesive
 76.2 - 102 microns3.00 - 4.00 milwith adhesive
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 17.2 MPa2490 psi
Peel Strength 0.701 kN/m4.00 pliAdhesion to Acrylic and uncoated, clear polycarbonate
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 16.0 °C>= 60.8 °FApplication Temperature
 
Descriptive Properties
AppearanceHolly Green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35070 / 169817

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.