  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Nioro™ Mac-Nioro™-WM Braze Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy; Solder/Braze Alloy

Material Notes: High-purity gold/copper/nickel alloy for vacuum brazing.

Applications:

  • Aero-engines (OEM and repair)
  • Aerospace fuel-line assemblies
  • Vacuum tubes
  • Wave guide and Klystron assemblies
  • Power supply surge arrestors
  • Automotive components

information provided by Morgan Advanced Materials

Key Words: Braze Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.567 lb/in³
Vapor Pressure 1.30 atm
@Temperature 800 °C
calculated
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 792 MPa
Elongation at Break 12 - 15 %2 in/50mm gage section
Compressive Yield Strength 686 MPa0.2% offset
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000275 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.5 µm/m-°C
@Temperature 20.0 - 850 °C
Thermal Conductivity 28.0 W/m-Kcalculated
Melting Point 950 - 950 °C
Solidus 950 °C
Liquidus 950 °C
 
Component Elements PropertiesOriginal ValueComments
Cadmium, Cd <= 0.0010 %
Gold, Au 82 %nominal
Lead, Pb <= 0.0020 %
Nickel, Ni 18 %nominal
Zinc, Zn <= 0.0010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Nioro™ ABA Mac-Nioro™ABA-WM Braze Alloy
Morgan Advanced Ceramics Paniro™ Mac-Palniro™7-WM Braze Alloy
Morgan Advanced Ceramics Nicoro™ Mac-Nicoro™-WM Braze Alloy
Morgan Advanced Ceramics 50Au-50Cu Mac-560Au/50 Cu-WM Braze Alloy
Morgan Advanced Ceramics Mac-35 Au/65 Cu-WM Braze Alloy

CMORF8002 / 203479

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.