MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Reliance Industries Relene B31101 Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Steel pipe coating base High Density Polyethylene resin.

Characteristics:broad molecular weight distribution, good melting strength, excellent toughness/ESCR, and good cut through/abrasion resistance.

Information provided by Reliance Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.943 g/ccASTM D1505
Environmental Stress Crack Resistance >= 400 hourF0; ASTM D1693/B
Oxidative Induction Time (OIT) >= 20 minASTM D3895
Melt Flow 0.28 g/10 min
@Load 2.16 kg
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
Tensile Strength, Yield 20.0 MPaASTM D638
Elongation at Break 800 %ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmASTM D257
Dielectric Constant 2.25ASTM D150
Dissipation Factor 0.000040ASTM D150
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 122 °CASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Reliance Industries Reclair F18010 Polyethylene
Reliance Industries Reclair O21010 Polyethylene
Reliance Industries Reclair O19010 Polyethylene
Reliance Industries Reclair M26500 Polyethylene
Reliance Industries Reclair M24300 Polyethylene

PREL074 / 65414

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.