MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huber Vertex® 100SP Magnesium Hydroxide
Categories: Ceramic; Oxide; Magnesium Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Vertex® magnesium hydroxide products provide excellent fire retarding and smoke suppression performance for thermoplastic, elastomeric and crosslinkable compounds. At 330°, they decompose in an endothermic reaction to form water and magnesium oxide. Vertex 100SP is a vinyl silane-treated product designed to provide excellent compounding rheology and high quality powder dispersion into such polymers as polyolefins, EPR/EPDM and other elastomers. Vertex 100SP is suitable for use in making fire-rated thermoplastic, elastomeric and crosslinkable compounds where use of high loading levels of the flame retardant is desired.

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.36 g/cc2.36 g/cc
Particle Size 1.1 µm1.1 µmSedigraph
 1.5 µm1.5 µmLaser Light Scattering
Particle Mesh Size 325 Mesh325 Mesh<0.5% Residue
Specific Surface Area 14 m²/g14 m²/gBET
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 2.52.5
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.581.58
 
Component Elements PropertiesMetricEnglishComments
Calcium, Ca <= 0.60 %<= 0.60 %
Free Water <= 0.50 %
@Temperature 105 °C
<= 0.50 %
@Temperature 221 °F
Free
Iron, Fe <= 0.080 %<= 0.080 %
Loss on Ignition(%) >= 31 %
@Temperature 1200 °C
>= 31 %
@Temperature 2190 °F
 
Descriptive Properties
ColorWhite
Content<0.3%Chloride
 >99%Mg(OH)2
FunctionalityLow Moisture Pick-Up
 Smoke Suppression
Market/Application: E & E, InfrastructureElectrical Switches, Connectors
Market/Application: ThermoplasticsYes
Market/Application: Wire and CableWire & Cable Jacketing - PVC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EHUBER795 / 300901

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.