MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lanxess Addocat® PP CASE Additive
Categories: Other Engineering Material; Catalyst/Initiator

Material Notes: Product Information: Addocat PP accelerates the drying and curing of 2-component polyurethane coatings based on aliphatic diisocyanates such as e.g. Desmodur N-types or Desmodur Z 4470 and polyols of the Desmophen series. The addition of Addocat PP reduces the pot life of the finish. To give greater convenience and accuracy of dosage, Addocat PP should be used as a 10% solution in solvents such as butyl acetate, ethyl acetate, methylisobutylketone, methylethylketone or xylene. The added quantity of Addocat PP is approx. 0.02 to 0.50% calculated on the total amount of Desmodur/Desmophen. The optimum dosage should be determined by trials.

Function: Catalyst for polyurethane coatings

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.870 g/cc0.0314 lb/in³
Water Absorption <= 0.50 %<= 0.50 %
Viscosity 3.0 cP3.0 cP
 
Thermal PropertiesMetricEnglishComments
Boiling Point 210 °C410 °FInitial
Pour Point -51.1 °C-60.0 °F
Flash Point 83.0 °C181 °FASTM D93, DIN EN 22719
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 15.0 - 25.0 °C
12.0 Month
@Temperature 59.0 - 77.0 °F
 
Descriptive Properties
Appearancecolorless to slightly yellowish, clear liquid
Content>24%Basic Nitrogen
Specifications>98%Active ingredient

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8198 / 208591

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.