MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RESPOL REPSOL PRIMEVA® P2850M EVA
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: Product Description: EVA copolymer REPSOL PRIMEVA® P2850M is a very low viscosity copolymer for hot melt adhesives applications. EVA resin REPSOL PRIMEVA® P2850M has been improved for a better stability against thermal degradation. It contains antioxidant and free flowing agent.
Applications: Hot Melt Adhesives – Packaging, Bookbinding, Pressure sensitive; Blends with waxes; Paper and cardboard coatings
Recommended melt temperature below 200°C to avoid the decomposition of the polymer. Processing conditions should be optimized for each production line.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: Antioxidant; Free Flowing Agent

Features: Antioxidant; Copolymer; Food Contact Acceptable; Good Thermal Stability; Low Viscosity

Uses: Adhesives; Blending; Packaging; Paper Coatings

Agency Ratings: EU Food Contact

Information provided by REPSOL

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.951 g/cc0.0344 lb/in³ISO 1183
Brookfield Viscosity 5000 cP
@Temperature 200 °C
5000 cP
@Temperature 392 °F
Spindle SC4-27
Vinyl Acetate Content 27.5 %27.5 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7171ISO 868
Tensile Strength at Break 1.80 MPa261 psiISO 527-2
Elongation at Break 130 %130 %ISO 527-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 67.8 °C154 °F
Ring & Ball Softening Point 82.2 °C180 °FASTM E28

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRESPOL1327 / 312020

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.