MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
Hapco SYMPOXY 1960G Epoxy system
Categories: Polymer; Thermoset; Epoxy

Material Notes: SYMPOXY 1960G is a single component epoxy system that is pigmented grey and has the following characteristics:
  • Flame Retardant to 94V-0
  • Excellent Moisture Resistance
  • Thermal Shock Resistant
  • Lightweight

Information provided by Hapco, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.350 - 0.400 g/ccASTM D-4669
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 12.0 ksiASTM D-695
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 8.30e+10 ohm-cmASTM D-270
Dielectric Constant 3.0to 10E6 cps; ASTM D-150
Dielectric Strength 480 V/milASTM D-149
Dissipation Factor 0.020to 10E6 cps; ASTM D-150
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.60 BTU-in/hr-ft²-°FASTM E-1225
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 150 °C
ASTM D-7750
 2.00 hour
@Temperature 125 °C
ASTM D-7750
 4.00 hour
@Temperature 85.0 °C
ASTM D-7750
 4.00 - 16.0 hour
@Temperature 90.0 °C
Demold
 
Descriptive Properties
Color (cured)Grey
Moisture Resistance0.03ASTM D-638
Weight Loss-0.005168 hrs @ 150°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHAPCO171 / 317230

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.