MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Stanyl® TE250F3 (DAM) Nylon 46 15% Glass Reinforced, Heat Stabilized, Flame Retardant (North America)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46); Nylon 46, Flame Retarded + Glass Fiber Reinforced

Material Notes: Information provided by DSM Engineering Plastics.

Former DSM Engineering Plastics product line is now with Envalior.

Key Words: Polyamide 46
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.52 g/ccISO 1183
Moisture Absorption at Equilibrium 2.1 %50% RH / 23°C; Similar to ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 140 MPaISO 527-1/-2
Elongation at Break 3.0 %ISO 527-1/-2
Tensile Modulus 8.00 GPaISO 527-1/-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
@Temperature 20.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature 20.0 °C
ISO 11359-1/-2
Melting Point 295 °CISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 290 °CISO 75-1/-2
UL RTI, Electrical 130 °C
@Thickness 1.50 mm
UL746B
Flammability, UL94 V-0
@Thickness 0.900 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eurotec® Tecomid® NT40 CR30 BK111 HS PPA, 30% carbon fiber reinforced, heat stabilized, natural
Envalior Stanyl® TW363 (COND) Nylon 46 Heat Stabilized, Impact Modified (North America)
Ensinger TECATOR™ TI 5013 Polyamide-imide (PAI)
RTP Company RTP 4087 A FR (Hot Water Moldable) Polyphthalamide (PPA), Carbon Fiber - Flame Retardant
Mitsubishi Chemical Advanced Materials Semitron™ ESd 520HR PTFE

PDSMA012 / 30948

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.