MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Ovako S400* S420N Steel, +AR
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: General Information: Grade SB400D is a micro-alloyed steel for general purposes with specified mechanical properties and impact requirements. The material is delivered as rolled and suitable for welding. The mechanical properties may change if the material is heat-treated. Grade SB420 is a micro-alloyed steel for general purposes with specified mechanical properties and impact requirements. The material is delivered as rolled. The mechanical properties may change if the material is heat-treated.

Information provided by Ovako

Key Words: 2142
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 160 - 205
@Thickness <=16.0 mm
Flat bar
 160 - 205
@Thickness 16.0 - 40.0 mm
Flat bar
 160 - 205
@Thickness 40.0 - 63.0 mm
Flat bar
 160 - 205
@Thickness 63.0 - 80.0 mm
Flat bar
 160 - 205
@Thickness 80.0 - 100 mm
Flat bar
Tensile Strength 520 - 680 MPa
@Thickness <=16.0 mm
Flat bar
 520 - 680 MPa
@Thickness 16.0 - 40.0 mm
Flat bar
 520 - 680 MPa
@Thickness 40.0 - 63.0 mm
Flat bar
 520 - 680 MPa
@Thickness 63.0 - 80.0 mm
Flat bar
 520 - 680 MPa
@Thickness 80.0 - 100 mm
Flat bar
Tensile Strength, Yield >= 360 MPa
@Thickness 80.0 - 100 mm
Rel, Flat bar
 >= 370 MPa
@Thickness 63.0 - 80.0 mm
Rel, Flat bar
 >= 390 MPa
@Thickness 40.0 - 63.0 mm
Rel, Flat bar
 >= 400 MPa
@Thickness 16.0 - 40.0 mm
Rel, Flat bar
 >= 420 MPa
@Thickness <=16.0 mm
Rel, Flat bar
Elongation at Break 18 %
@Thickness 63.0 - 80.0 mm
Flat bar
 18 %
@Thickness 80.0 - 100 mm
Flat bar
 19 %
@Thickness <=16.0 mm
Flat bar
 19 %
@Thickness 16.0 - 40.0 mm
Flat bar
 19 %
@Thickness 40.0 - 63.0 mm
Flat bar
Modulus of Elasticity 210 GPa
Poissons Ratio 0.30
Shear Modulus 80.0 GPa
Impact Test 40.0 J
@Thickness <=16.0 mm,
Temperature -20.0 °C
Flat bar
 40.0 J
@Thickness 16.0 - 40.0 mm,
Temperature -20.0 °C
Flat bar
 40.0 J
@Thickness 40.0 - 63.0 mm,
Temperature -20.0 °C
Flat bar
 40.0 J
@Thickness 63.0 - 80.0 mm,
Temperature -20.0 °C
Flat bar
 40.0 J
@Thickness 80.0 - 100 mm,
Temperature -20.0 °C
Flat bar
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 40.0 - 45.0 W/m-KAmbient temperature
Transformation Temperature 400 °CMS
 720 °CAC1
 820 °CAC3
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.020 %
Carbon, C <= 0.20 %
Copper, Cu <= 0.55 %
Iron, Fe 96.51 - 98.92 %As Balance
Manganese, Mn 1.0 - 1.7 %
Molybdenum, Mo <= 0.10 %
Nickel, Ni >= 0.080 %
Nitrogen, N <= 0.025 %
Phosphorus, P <= 0.035 %
Silicon, Si <= 0.60 %
Sulfur, S <= 0.030 %
Titanium, Ti <= 0.030 %
Vanadium, V <= 0.20 %
 
Descriptive Properties
WeldabilityCEV 0.6max
 Pcm 0.35max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ThyssenKrupp PAS 420 Structural Steel for Cold Forming
JIS SPHC Nonresulfurized Carbon Steel

NOVAKO425 / 234724

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.