MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Special Metals BRIGHTRAY® Alloy F Electrical Resistance Alloy  (discontinued **)
Categories: Metal; Electronic/Magnetic Alloy; Superalloy; Iron Base

Material Notes: A nickel-iron-chromium electrical-resistance alloy for use at temperatures up to 1920°F (1050°C) under continuous operating conditions. Its high iron content and relatively low level of nickel make it particularly resistant to internal oxidation in atmospheres that alternate between oxidizing and reducing or carburizing. The alloy has a high temperature coefficient of resistance. Used for heating elements in industrial furnaces. Standard product forms are sheet and strip.

Data provided by the manufacturer, Special Metals.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.86 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 690 MPa100000 psiAnnealed prior to test
 540 MPa
@Temperature 550 °C
78300 psi
@Temperature 1020 °F
Annealed prior to test
Tensile Strength, Yield 370 MPa
@Strain 0.2 %
53700 psi
@Strain 0.2 %
Annealed prior to test
 270 MPa
@Strain 0.2 %,
Temperature 550 °C
39200 psi
@Strain 0.2 %,
Temperature 1020 °F
Annealed prior to test
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000108 ohm-cm0.000108 ohm-cmTemperature coefficient of resistance is 290 µOhm/Ohm-°C in the range 25-500°C.
Magnetic Permeability 1.0381.038at 200 Oersted (15.9 kA/m)
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.0 µm/m-°C
@Temperature 20.0 - 100 °C
8.33 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.450 J/g-°C0.108 BTU/lb-°F
Melting Point 1330 - 1400 °C2430 - 2550 °F
Solidus 1330 °C2430 °F
Liquidus 1400 °C2550 °F
Maximum Service Temperature, Air 1050 °C1920 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.050 %0.050 %
Chromium, Cr 18 %18 %
Iron, Fe 42 %42 %
Manganese, Mn 1.2 %1.2 %
Nickel, Ni 37 %37 %
Silicon, Si 2.3 %2.3 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carpenter Chrome Core® 18-FM Solenoid Quality Stainless Steel, Annealed
Carpenter Chrome Core® 8 Alloy
Carpenter Glass Sealing "42-6" Alloy
ETREMA Products Terfenol-D Magnetostrictive Smart Material (Tb0.3Dy0.7Fe1.92)
H.C. Starck Ampersint® MAP FeNi 50/50 For Soft Magnets

NIND12 / 17521

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.