UTS50 12K is a family of ultra-high tenacity aerospace grade carbon fibers made in Japan for use as reinforcements in high performance composites. These fibers are produced from poly-acrylonitrile (PAN) precursor and are surface treated to promote adhesion to organic matrix polymers. Sizing materials are designed to aid in handling.Information provided by Teijin Carbon America, Inc. |