MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Traid Villarroya TRAIDAMID® E Nylon 6, Extruded
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Extruded

Material Notes:
  • Very abrasion resistant
  • Electrically insulating
  • Good chemical resistance to many oils, diesel, petrol and greases
  • Tough and rigid
  • Easy machined
Industry Applications:
  • Impact and damping plates
  • Conveyor screws
  • Friction bearings
  • Castors
  • Gear wheels

Information provided by Traid Villarroya Hnos. S.L.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³
Water Absorption 3.0 %
@Time 86400 sec
3.0 %
@Time 24.0 hour
DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 160 MPa23200 psiISO 2039-1
Tensile Strength, Yield 85.0 MPa12300 psi50 mm/min; DIN EN ISO 527-2
Elongation at Break 70 %70 %50 mm/min; DIN EN ISO 527-2
Creep Strength 45.0 MPa
@Time 3.60e+6 sec
6530 psi
@Time 1000 hour
with static load
Modulus of Elasticity 3.00 GPa435 ksi1 mm/min; DIN EN ISO 527-2
Charpy Impact Unnotched NBNBMax. 7,5j; DIN EN ISO 179-1EU
Coefficient of Friction 0.38 - 0.450.38 - 0.45Against steel p=0,05 N/mm2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmDIN IEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmDIN IEC 60093
Dielectric Constant 3.7 - 7.0
@Frequency 100000 Hz
3.7 - 7.0
@Frequency 100000 Hz
DIN 53483
Dielectric Strength 20.0 - 50.0 kV/mm
@Thickness 1.00 mm
508 - 1270 kV/in
@Thickness 0.0394 in
ASTM 149
Dielectric Loss Index 0.031 - 0.30
@Frequency 100000 Hz
0.031 - 0.30
@Frequency 100000 Hz
DIN 53483
Comparative Tracking Index 600 V600 VDIN 53480
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FDIN 53483
Specific Heat Capacity 1.70 J/g-°C0.406 BTU/lb-°FISO 22007-4:2008
Thermal Conductivity 0.230 W/m-K1.60 BTU-in/hr-ft²-°FISO 22007-4:2008
Melting Point 220 °C428 °FDIN 53765
Maximum Service Temperature, Air 100 °C212 °FLong term
 160 °C320 °FShort term
Glass Transition Temp, Tg 60.0 °C140 °FDIN 53765
Flammability, UL94 HBHBDIN IEC 60995-11-10
 
Descriptive Properties
ColorNatural opaque
Resistance to hot mater / basesLimited
Resistance to weatheringNot resistant
Time yield limit for 1% elong4.5 MPaAfter 1000 hours

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAID900 / 318861

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.