MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Meyors Chemical Rubber Accelerator CBS (CZ)
Categories: Other Engineering Material

Material Notes: Product Code: MSHQD-AC005-00 OT
Chemical Name: N-Cyclohexyl-2-benzothiazolesulfenamide
Trade Name: Rubber Accelerator CBS (CZ)
CAS No.: 95-33-0
Molecular Formula: C13H16N2S2

Typical Properties: Grayish-white powder with little odor, no poison. The density is 1.31-1.34. The melting point is more than 96?.Soluble in Toluene, Chloroform, benzene, CS2, CH2Cl2, acetone, ethyl acetate, insoluble in water, gasoline, acid/Alkali with lower concentration.

Recommended Applications: In industrial rubber products. CBS can be used with secondary accelerators, like as the TMTD to replace MBTS/DPG systems. CBS can also be used in EPDM and NBR compounding as the primary accelerator, giving good scorch delay and fast cure rates. CBS can be (in combination with CTP) used as an alternative for NOBS. It can avoid the problem caused by N-nitrosamines. And it also has the equal function on scorch safety and faster cure rate as NOBS

Information provided by Meyors Chemical INC Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Molecular Weight 264.4 g/mol
Ash <= 0.30 %
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 96.0 °CInitial
 
Descriptive Properties
AppearanceLight yellow powder
Content<0.1%Residues (150µm)
 1-2%Oil
Insoluble in methanol<0.5%
Loss on drying<0.4%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMEYORS001 / 316583

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.