MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Marco Polo MARPOL LDF 701-B Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: MARPOL® LDF 701-B is a homopolymer film resin with great clarity and stiffness. Film made from this resin may be used in overwrap applications and in push-through type packaging equipment.

Recommended Applications: Bread bags, co-extrusion films, collation shrink, diaper backsheets, frozen food packaging, high performance collation, shrink, hygiene packaging, label film, laminating film and overwrap paper and film, pallet shrink film, medium duty shrink film.

Additives: antiblock – 3000 ppm, slip – no

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ASTM D1505
Melt Flow 0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 3000 ppm3000 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 11.0 MPa1600 psiASTM D882
Film Tensile Strength at Yield, TD 11.7 MPa1700 psiASTM D882
Film Elongation at Break, MD 130 %130 %ASTM D882
Film Elongation at Break, TD 540 %540 %ASTM D882
Flexural Modulus, 1% Secant 235 MPa34100 psiMD; ASTM D882
 290 MPa42100 psiTD; ASTM D882
Elmendorf Tear Strength MD 510 g510 gASTM D1922
Elmendorf Tear Strength TD 140 g140 gASTM D1922
Dart Drop Test 160 g0.353 lbASTM D1709
Film Tensile Strength at Break, MD 25.5 MPa3700 psiASTM D882
Film Tensile Strength at Break, TD 22.1 MPa3200 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 113 °C235 °FPeak; ASTM D3418
 
Optical PropertiesMetricEnglishComments
Haze 9.6 %9.6 %ASTM D1003
Gloss 57 %57 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMARCO095 / 283692

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.