MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Phon Tech PHOENIX™ 04501 Blow Molding Grade TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Blow molding is a manufacturing process by which hollow plastic parts are formed. In general, there are three main types of blow molding: extrusion blow molding, injection blow molding, and injection stretch blow molding. Mostly the TPEs parts are manufactured by extrusion blow molding. The process starts with melting TPEs into tube. The tube is clamped into a blow molding mold. The tube is pinched at one end, welding it together and then air is blown into it. The air inflates the TPEs out to match the mold cavity. Once the TPEs has cooled down and hardened, the mold opens and the part is ejected. Phon Tech has developed PHOENIX™ Blow Molding Grade Thermoplastic Elastomers (TPEs) that are suitable for blow molding process. They can be used for medical balloon tamponade, BP cuff balloon, dropper suction, blower bulb, toy, automotive bellow, etc.

Features:

  • Smooth and silky surface
  • Non-sticky
  • Excellent tensile strength
  • Excellent resilience
  • Stable melt flow
Applications: Blown film, BP cuffballoon, toys, medical balloon tamponade, blower bulb, etc.

Information provided by Phon Tech Industrial Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.850 - 0.910 g/cc0.850 - 0.910 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 52 - 5852 - 58ASTM D2240
Tensile Strength 8.9811 MPa1302.6 psiASTM D412
Elongation at Break 1120.7 %1120.7 %ASTM D412
100% Modulus 1.460 MPa211.8 psiASTM D412
Tear Strength 32.13 kN/m183.3 pliASTM D624 Die C
 
Descriptive Properties
ColorTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPHONT101 / 296443

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.