MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPV 14065 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 14065B BLK is a low density, medium hardness thermoplastic vulcanizate that is designed specifically for demanding automotive and industrial applications. It exhibits excellent compression set, flex fatigue, high and low temperature performance. This product can be processed by injection molding, blow molding and extrusion for applications such as seals, gaskets, chemical resistant hose and tube, boots and bellows.

Availability: Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Excellent Elastic Recovery; Fatigue Resistant; Good Adhesion; Good Flexibility; Mold Moldability; Good Processability; Good Surface Finish; High Melt Stability; Low Density; Medium Hardness; Medium Heat Resistance; Resilient

Uses:Automotive Components; Automotive Applications; Automotive Exterior Parts: Automotive Interior Parts; Automotive Under the Hood; Blow Molding Applications; Gaskets; Grommets; Hose; Industrial Applications; O-rings: Pipe Seals; Plugs; Rubber Replacement; Seals; Tubing; White Goods & Small Appliances

Agency Ratings: UL QMFZ2; UL QMFZ8

Automotive Specifications: BMW Unspecified Color: Black; CHRYSLER MS-AR-100 BGN Color: Black; CHRYSLER MS-AR-100 BGN Color: Natural; FORD WSD-M2D378-A6 Color: Black; FORD WSD-M2D378-A6 Color: Natural; GM GMP.E/P.002 Color: Black; GM GMP.E/P.002 Color: Natural; GM GMW15813 Type 5 Color: Black; GMW15813 Type 5 Color: Natural; GM QK 3521 Type 1 Color: Black ; GM QK 3521 Type 1 Color: Natural

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding: Blow Molding: Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.942 g/cc0.0340 lb/in³ISO 1183
 0.944 g/cc0.0341 lb/in³ASTM D792
Viscosity 305 cP
@Shear Rate 206 1/s,
Temperature 200 °C
305 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  63
@Time 5.00 sec
63
@Time 0.00139 hour
Extruded; ASTM D2240
 65
@Time 5.00 sec
65
@Time 0.00139 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 7.03 MPa1020 psiAcross Flow; ISO 37
 6.26 MPa
@Treatment Temp. 150 °C,
Time 605000 sec
908 psi
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 6.40 MPa
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
928 psi
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain 2.60 MPa
@Strain 100 %
377 psi
@Strain 100 %
Across Flow; ISO 37
 2.60 MPa
@Strain 100 %,
Treatment Temp. 135 °C
377 psi
@Strain 100 %,
Treatment Temp. 275 °F
Across Flow, Change in Air at 1000 hr; ISO 188
 2.70 MPa
@Strain 100 %,
Treatment Temp. 150 °C
392 psi
@Strain 100 %,
Treatment Temp. 302 °F
Across Flow, Change in Air at 168 hr; ISO 188
Elongation at Break 650 %650 %Across Flow; ISO 37
 579 %
@Treatment Temp. 150 °C,
Time 605000 sec
579 %
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 598 %
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
598 %
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air; ISO 188
Tear Strength 29.1 kN/m166 pliAcross Flow; ASTM D624
 29.8 kN/m170 pliMethod Ba, Angle (Unnicked), Across Flow; ISO 34-1
Compression Set 35 %
@Temperature 70.0 °C,
Time 79200 sec
35 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -65.0 °C-85.0 °FASTM D746
UL RTI, Electrical 100 °C212 °FUL 746
UL RTI, Mechanical with Impact 65.0 °C149 °FUL 746
UL RTI, Mechanical without Impact 100 °C212 °FUL 746
Flammability, UL94 HB
@Thickness 1.02 mm
HB
@Thickness 0.0400 in
All Colors
 
Processing PropertiesMetricEnglishComments
Processing Temperature 187 - 220 °C369 - 428 °FInjection
Rear Barrel Temperature 180 - 215 °C356 - 419 °FInjection
Middle Barrel Temperature 180 - 215 °C356 - 419 °FInjection
Front Barrel Temperature 180 - 215 °C356 - 419 °FInjection
Nozzle Temperature 187 - 220 °C369 - 428 °FInjection
Zone 1 180 - 200 °C356 - 392 °FExtrusion
Zone 2 180 - 210 °C356 - 410 °FExtrusion
Zone 3 180 - 210 °C356 - 410 °FExtrusion
Zone 4 180 - 210 °C356 - 410 °FExtrusion
Die Temperature 195 - 215 °C383 - 419 °FExtrusion
Melt Temperature 195 - 215 °C383 - 419 °FExtrusion
Mold Temperature 10.0 - 55.0 °C50.0 - 131 °FInjection
Drying Temperature 82.2 °C180 °F
Dry Time 3.00 hour3.00 hour
Screw Speed 100 - 200 rpm100 - 200 rpmInjection
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1177 / 237668

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.