MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

Plansee ML Molybdenum-Lanthanum Oxide Rod
Categories: Metal; Nonferrous Metal; Molybdenum Alloy; Refractory Metal

Material Notes: Characteristics:
  • "Stacked fiber" microstructure
  • Extremely creep resistant

Applications:

  • Furnace components - wires, including stranded; sintering and annealing boats; evaporator coils
  • Lighting - retaining and feed wires

Information provided by Plansee.

Vendors: PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 2000 °C3630 °FMicrostructure stable up to this point
 
Processing PropertiesMetricEnglishComments
Recrystallization Temperature 1300 °C2370 °FDeformation level - 90%
 2000 °C3630 °FDeformation level - 99.99%
 
Component Elements PropertiesMetricEnglishComments
Molybdenum, Mo 99.7 %99.7 %Balance
Other, each 0.30 %0.30 %Lanthanum Oxide
 
Descriptive Properties
Creep Resistance< 1400°Cmuch greater than pure Mo
Ductilitymuch greater than pure Moafter HT use
Stability at High Temperature> 1400°Cgreater than pure Mo
Stability at Room Temperaturecomparable with pure Mo
Weldabilitygreater than pure Mo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
California Fine Wire Nickel A 200 Nickel Alloy
Schwarzkopf Plansee PM 2000, Bar Grain Class 6 ODS Iron Alloy Bar
Datum Alloys Nickel 200/201 Strip and Tags
W-26Re Tungsten-Rhenium Thermocouple Alloy
Brandenburger S 5000 Ablation Material for Aeronautics and Space Aviation

NPLAM903 / 135459

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.