MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Polyplastic Compounds Tehnamid® A-SV25-ETK Nylon 66, 25% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: 25% glass fiber reinforced polyamide 66 with increased thermal stability, extruded. Designed for the manufacture by extrusion of products used in various industries, including for thermally insulating profiles. Serially produced in natural and black.

Information provided by Polyplastic Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³GOST 15139
Water Absorption 0.80 %
@Time 86400 sec
0.80 %
@Time 24.0 hour
GOST 4650
Linear Mold Shrinkage, Flow 0.0015 - 0.0035 cm/cm0.0015 - 0.0035 in/inGOST 18616
Linear Mold Shrinkage, Transverse 0.0090 - 0.012 cm/cm0.0090 - 0.012 in/inGOST 18616
Melt Flow 2.0 - 5.0 g/10 min
@Load 2.16 kg,
Temperature 275 °C
2.0 - 5.0 g/10 min
@Load 4.76 lb,
Temperature 527 °F
GOST 11645
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 140 MPa20300 psiGOST 11262
Elongation at Break 4.5 %4.5 %GOST 11262
Flexural Strength 205 MPa29700 psiat maximum load; GOST 4648
Flexural Modulus 6.80 GPa986 ksiGOST 9550
Charpy Impact Unnotched  5.70 J/cm²
@Temperature -40.0 °C
27.1 ft-lb/in²
@Temperature -40.0 °F
GOST 4647
 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
GOST 4647
Charpy Impact, Notched  1.10 J/cm²
@Temperature -40.0 °C
5.23 ft-lb/in²
@Temperature -40.0 °F
GOST 4647
 1.40 J/cm²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
GOST 4647
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+12 ohm-cm2.00e+12 ohm-cmGOST 6433.2
Dielectric Strength 35.0 kV/mm889 kV/inGOST 6433.3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 25.0 µm/m-°C13.9 µin/in-°FGOST 15173
Melting Point 255 °C491 °FGOST 21553
Deflection Temperature at 0.46 MPa (66 psi) 254 °C489 °FGOST 12021
Deflection Temperature at 1.8 MPa (264 psi) 235 °C455 °FGOST 12021

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLPLC125 / 307197

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.