MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Tritan™ Renew TX2001-50 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Tritan™ Renew TX2001-50 is an amorphous copolyester with excellent appearance and clarity. Tritan Renew TX2001-50 contains a mold release derived from vegetable based sources. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistance. This new-generation copolyester can also be molded into various applications without incorporating high levels of residual stress. Combined with Tritan's outstanding chemical resistance and hydrolytic stability, these features give molded products enhanced durability in the dishwasher environment, which can expose products to high heat, humidity, and aggressive cleaning agents. Tritan Renew TX2001-50 may be used in repeated use food contact articles under United States Food and Drug Administration (FDA) regulations. Tritan Renew TX2001-50 is certified to NSF/ANSI Standard 51 for Food Equipment Materials. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Applications

  • Appliances (food contact)
  • Consumer electronics
  • Consumer housewares - food contact (fc)
  • Consumer housewares-nfc
  • Large appliances non-food contact
  • Lighting
  • Packaging components non food contact
  • Personal care & cosmetics packaging
  • Process additives
  • Tools
  • Toys
  • Water/sport bottles
Key Attributes
  • Ease of processing
  • Excellent clarity
  • Excellent hydrolytic stability
  • Fast drying times
  • Good chemical resistance
  • Good heat resistance
  • Outstanding impact resistance
  • Quick cycle times

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ASTM D792
Linear Mold Shrinkage 0.00500 - 0.00700 cm/cm0.00500 - 0.00700 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115115ASTM D785
Tensile Strength at Break 49.0 MPa7110 psiISO 527
 53.0 MPa7690 psiASTM D638
Tensile Strength, Yield 44.0 MPa6380 psiASTM D638
 45.0 MPa6530 psiISO 527
Elongation at Break 130 %130 %ISO 527
 140 %140 %ASTM D638
Elongation at Yield 7.00 %7.00 %ISO 527
 7.00 %7.00 %ASTM D638
Tensile Modulus 1.585 GPa229.9 ksiASTM D638
 1.624 GPa235.5 ksiISO 527
Flexural Yield Strength 66.0 MPa9570 psiASTM D790
Flexural Modulus 1.531 GPa222.1 ksiISO 178
 1.585 GPa229.9 ksiASTM D790
Izod Impact, Notched 6.50 J/cm12.2 ft-lb/inASTM D256
Izod Impact, Unnotched NBNBASTM D4812
Izod Impact, Notched (ISO)  14.0 kJ/m²
@Temperature -40.0 °C
6.66 ft-lb/in²
@Temperature -40.0 °F
ISO 180
 66.0 kJ/m²
@Temperature 23.0 °C
31.4 ft-lb/in²
@Temperature 73.4 °F
ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 109 °C228 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C198 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Haze <= 1.00 %<= 1.00 %ASTM D1003
Transmission, Visible 92.0 %92.0 %Total; ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 282 °C500 - 540 °F
Mold Temperature 38.0 - 66.0 °C100 - 151 °F
Drying Temperature 88.0 °C190 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details
NSF YesYesSee notes for details

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM4227 / 323850

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.