MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Syensqo (Solvay Specialty Polymers) Kyton P002CQ Polyphenylene Sulfide (PPS)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Kyton P002CQ Fiber Grade Resins are high molecular weight polyphenylene sulfide polymers suitable for monofilament and/or multifilament fiber extrusion. They exhibit excellent thermal stability and chemical resistance.

Key Attributes: Chemical Resistant; Good Thermal Stability; High Molecular Weight

Applications: Fibers

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ASTM D792
Volatiles 0.30 %0.30 %
Water Absorption at Saturation 0.050 %0.050 %ASTM D570
Melt Flow 100 g/10 min
@Load 5.00 kg,
Temperature 316 °C
100 g/10 min
@Load 11.0 lb,
Temperature 601 °F
Procedure B; ASTM D1238
Ash 0.30 %0.30 %ISO 3451-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 85.0 MPa12300 psiASTM D638
Elongation at Break 10 %10 %ASTM D638
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 24.0 kV/mm610 kV/inASTM D149
Dissipation Factor 0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
27.8 µin/in-°F
@Temperature -58.0 - 122 °F
ASTM E831
Melting Point 285 °C545 °FISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °FUnannealed; ASTM D648
 
Descriptive Properties
Availability (as of March 2019)Africa & Middle East; Asia Pacific; Europe; Latin America; North America
FormsPellets
ProcessingFilament Extrusion
RoHS ComplianceRoHS Compliant

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y5248 / 238629

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.