MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nouryon Perkadox BTW-50 Dibenzoyl peroxide, paste, 50% in dipropylene glycol dibenzoate and water
Categories: Other Engineering Material

Material Notes: Perkadox BTW-50 is the preferred BPO paste for unsaturated polyester & vinyl ester resins.

CAS number: 94-36-0

EINECS/ELINCS No.: 202-327-6

Applications: Perkadox BTW-50 is a paste containing 50% dibenzoyl peroxide without phthalate for the curing of unsaturated polyester resins at ambient and elevated temperatures. At temperatures up to 80°C, Perkadox BTW-50 should be used in combination with an aromatic tertiary amine accelerator, above 80°C the use of an accelerator is not required. Perkadox BTW-50 has primarily been developed for the putty market. For non filled systems, Perkadox CH 50X or Perkadox 40E are better applicable with respect to miscibility with the UP resin. Perkadox BTW-50 shows a very good chemical and physical stability and is therefore very suitable for tube filling. The curing system Perkadox BTW-50/amine accelerator shows a very fast cure that is hardly influenced by humidity and fillers. Even at low temperatures a relatively good cure will be obtained. A disadvantage may be the yellow color and poor light resistance of the moulded product.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
Molecular Weight 242.2 g/mol242.2 g/mol
Storage Temperature <= 25.0 °C<= 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 50.0 °C122 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceWhite homogeneous paste
Assay48.5-51.0 %
Content (%)6.61Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY804 / 286327

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.