Isocor™ HG20SC us a medium viscosity compounding grad PA-612 based nylon. This resin is specifically suited for applications requiring lower moisture regain and greater dimensional stability. Isocor™ HG20SC is used in applications requiring good electrical insulation properties. This resin can be processed with conventional techniques. Used for injection molding, automotive, lawn and garden, tubing, and films. Information provided by Shakespeare Company. |