MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Pyrotek TS-103 Thermoset Electrical Insulation Product (Nema Grade: G-3)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes: Glass reinforcement, Phenolic resin, Natural color. Good heat resistance. Excellent mechanical and machining properties.

Applications

  • Superstructure support pads
  • Bus bar insulators
  • Pot cradle insulators
  • Exhaust duct insulators
  • Machined parts
  • Wedges & shunts
  • Point feeder gaskets

Advantages

  • High insulation properties
  • High strength
  • Low moisture absorption
  • High temperature resistance

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.794 g/cc0.06481 lb/in³
Water Absorption 0.50 %0.50 %
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 345 MPa50000 psi
Compressive Strength 310 MPa45000 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.30e+10 ohm-cm1.30e+10 ohm-cm
Dielectric Strength 16.0 kV/mm406 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C351 °FContinuous

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek O'-Sialon Non-Oxide Ceramic
Pyrotek S-679 Dense Graphite Material Treated for Oxidation Resistance
Pyrotek Valcor® G Pre-Cast Shapes
Pyrotek Valcor® G-AZ Pre-Cast Shapes
Pyrotek Pyrite N-14 Refractory Board

PPYRO058 / 58391

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.