Description: TECKBOND-NC is a silicone rubber base filled with nickel coated graphite particles to produce a highly conductive one-component adhesive sealant. The system is an RTV moisture-cured compound which is ready to use without additional preparation or mixing. The compound cures at room temperature to form a flexible resilient conductive bond or sealant. Application Information: TECKBOND conductive adhesive-sealants are recommended wherever a flexible bond is required in a metal-to-silicone gasket application, such as TECKNIT NC-CONSIL®. Information provided by Chomerics |