MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ExxonMobil LDPE LD 600BA Low Density Polyethylene Resin (European Grade)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: LD 600BA is a high flow LDPE grade, characterized by high stiffness and good toughness. It’s easy processable.

Availability: Africa & Middle East and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: No
Applications:
  • Caps
  • Closures
  • Compounding
  • Food Packaging Containers
  • Houseware Articles
  • Injection Molding
  • Masterbatch Base Resin
  • Technical Parts
  • Toys
  • Viscosity Modifier

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccExxonMobil method
Melt Flow 21 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 44ISO 868
Tensile Strength at Break 1300 psiISO 527-2/1A/50
Elongation at Break 140 %ISO 527-2/1A/50
Tensile Modulus 28000 psiISO 527-2/1A/1
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 228 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 196 °FISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow LDPE 955I Low Density Polyethylene
Dow LDPE 510I Low Density Polyethylene
LyondellBasell Lupolen 1810 H LDPE, Injection Molding Grade
Envalior Novamid® 3021GH30 NAT PA66-GF30
Dow 650I Low Density Polyethylene Resin

PEX99282 / 175518

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.