MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Trelleborg Emerson & Cuming Eccobond® 45 Two-Component General Purpose Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Emerson & Cuming 45 Eccobond® Two-Component General Purpose Epoxy Adhesive
Filled, general purpose, room temperature curing, epoxy adhesive and sealant. Flexibility can be adjusted by the amount of Catalyst 15 used. Convenient mix ratio. Good impact resistance. Excellent adhesion to metal, glass and plastic substrates. Mix Ratio of 100:50 to 100:150 (Cat 15 variation). Bonding Type: Epoxy

The Eccobond® product line is now a part of Henkel; this specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 - 1.34 g/cc
Viscosity 37000 cP
@Temperature 25.0 °C
Mixed
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 3100 psi
 
Processing PropertiesOriginal ValueComments
Cure Time 0.250 hour
@Temperature >=105 °C
 0.500 hour
@Temperature 70.0 °C
 24.0 hour
@Temperature 25.0 °C
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trelleborg Emerson & Cuming Eccobond® 285 Two-Component Thermally Conductive Epoxy Adhesive
CHT Group QM 245 QSI Quantum Silicones 45 Durometer Addition Cure Moldmaking Material

PEMERS47 / 35739

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.