MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo LGF 9621 Homopolymer Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Overview: LGF 9621 is polypropylene homopolymer reinforced with 60% by weight of long glass fibers. (PP-LGF60, Long Glass fiber Granulate). This PP-LGF60 is a ‘concentrate’ which has to be diluted with either ‘neat’-polypropylene and/or mineral filled PP based compounds. The ‘dilution’ is typically done as a dry blend of granulates by means of gravimetric dosing devices at the injection-molding machine. A weight ratio of 1:2 of LGF 9621.00 and i.e. LGF 8100 PP-copolymer will result in a composite-system have 20% by weight of glass fibers. LGF 9621 has been especially formulated to meet the long term heat ageing resistance (LTHA) required for use in some automotive ‘interior’ applications i.e. instrument panel carrier or integrated door-modules. LTHA > 100 h@140°C and/or LTHA > 400 h @150°C will be achieved after dilution to 20% GF-content with ‘neat’-PP (LGF 8000 or LGF 8100). The ‘long’ glass fibers (11mm length) provide high stiffness, strength and impact-resistance of the injection molded parts. The properties shown below have been measured on standardized ‘dong bone’ –shape specimens (ISO 3167). Note” The mechanical properties which will be present in ‘real’ injection-molded parts may be different – depending on the fiber-orientation and the fiber-length distribution profile – which themselves are resulting from hardware configuration and processing parameters (such as i.e. the type of screw and mixing elements, diameter and radii of nozzle and hot-runners, number and size of gates, injection speed during mold filling and backpressure during dosing cycle.)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 105 MPaISO 527-2/50
Elongation at Break 2.3 %ISO 527-2/50
Tensile Modulus 6500 MPaISO 527-2
Flexural Strength 155 MPa3-Point Bending; ISO 178
Flexural Modulus 6500 MPa3-Point Bending; ISO 178
Flexural Strain at Break 3.0 %outer 'fiber' strain; ISO 178
Charpy Impact Unnotched 45.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1fU
 53.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1fU
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 156 °CUnannealed; ISO 75-2/A

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostacom™ 62F4-2C Polypropylene Homopolymer
Multibase Multi-Pro® 1012 C BLK Medium Impact Mineral Filled Polypropylene
Synthos DLGF9411.00 Polypropylene
Trinseo INSPIRE™ DLGF 9631.01 Z Polypropylene homopolymer, 60% LGF
Cossa Polimeri ESTAPROP H 10100 BS Polypropylene, 50% Mineral Filled

PZZDWST082 / 142291

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.