A Terpolymer of high molecular weight, moderate ethylene content and medium diene level. Produced with ExxonMobil Chemical proprietary technology offering bimodal molecular weight distribution. The polymer is supplied in semi-friable bales to facilitate single-pass mixing. Information provided by ExxonMobil Chemical |