MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SSAB Tunnplat Domex® 420MC HSLA Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel

Material Notes: HSLA Steel

Characteristics: Some thicknesses of these steel grades are available with a maximum of 0.03% Si for thin Zn coating. If the material is to be hot-dip galvanized and steel with a maximum Si content of 0.03% is not available, the silicon content should be 0.2%..

Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better properties.

Property data is for hot-rolled steel.

Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex® high strength steels offers a number of benefits compared to ordinary structural steels: Lower weight, Simpler production, Lower creep rate, Longer useful life, Higher load-bearing capacity, Lower transport costs, Reduced stocks, Lower overall cost.

Data provided by SSAB Tunnplat.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³Estimated by MatWeb
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 480 - 620 MPa69600 - 89900 psi
Tensile Strength, Yield >= 420 MPa>= 60900 psi
Elongation at Break  >= 16 %
@Thickness <=3.00 mm
>= 16 %
@Thickness <=0.118 in
A80
 >= 20 %
@Thickness >=3.00 mm
>= 20 %
@Thickness >=0.118 in
A5
Bend Radius, Minimum >= 0.50 t>= 0.50 tt<3mm; internal bend radius, 90°
 >= 1.0 t>= 1.0 t3 mm < t< 6mm; internal bend radius, 90°
 >= 1.0 t>= 1.0 tt>6mm; internal bend radius, 90°
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al >= 0.015 %>= 0.015 %
Carbon, C <= 0.10 %<= 0.10 %
Iron, Fe 98 %98 %As remainder
Manganese, Mn <= 1.5 %<= 1.5 %
Niobium, Nb (Columbium, Cb) <= 0.090 %<= 0.090 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si <= 0.30 %<= 0.30 %
Sulfur, S <= 0.010 %<= 0.010 %
Titanium, Ti <= 0.15 %<= 0.15 %
Vanadium, V <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SSAB Tunnplat Domex® 355MC HSLA Steel
SSAB Tunnplat Domex® 315MC HSLA Steel
SSAB Tunnplat Domex® 460MC HSLA Steel
SSAB Tunnplat Domex® 500MC HSLA Steel
A. Schulman Diamond ABS 3501 Black 1302 Injection Molding Grade

NTUNN19 / 19511

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.