MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Total PPH 3576 BB Polypropylene Homopolymer, Cast Film
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Polypropylene 3576 BB is recommended for use in non-oriented cast films processes. It contains an optimized level of slip and anti-block additives.

3576 BB is intended for food, magazine or textile packaging, for lamination films as well as for stationary supplies.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.525 g/ccISO 1183
Melt Flow 8.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
Antiblock Level 1800 ppmSiO2
Slip Level 1800 ppmErucamide
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 30.0 MPaASTM D638
Flexural Modulus 1400 MPaASTM D790
Izod Impact, Notched 35.0 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CDSC
Vicat Softening Point 153 °C
@Load 1.02 kg
ASTM D1525
 
Descriptive Properties
Isotacticity Index (%)97.5Total Internal Test

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTOTAL803 / 130528

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.