MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ampco Metal AMPCOLOY® 712 Tin Bronze, Castings
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze; Copper Casting Alloy

Material Notes: Alloy used primarily for its excellent mechanical and corrosion resistance. Specific pressure up to 60 MPa. Linear speed up to 6 m/sec.

Applications: Spindle screw; Pressure screw-nut; Gear wheel; Machine tool parts

Key Words: CDA C 91700; DIN 1705 CuSn12Ni 2.1052.04; DIN 1705 CuSn12Ni 2.1052.03; DIN 1705 CuSn12Ni 2.1052.01
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.60 g/cc0.311 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 8080HB 10
Tensile Strength, Ultimate 260 MPa37700 psi
Tensile Strength, Yield 140 MPa
@Strain 0.2 %
20300 psi
@Strain 0.2 %
Elongation at Break 12 %12 %
Modulus of Elasticity 118 GPa17100 ksi
 
Component Elements PropertiesMetricEnglishComments
Antimony, Sb <= 0.20 %<= 0.20 %
Copper, Cu 84 - 88.5 %84 - 88.5 %
Lead, Pb 1.0 %1.0 %
Nickel, Ni 2.0 %2.0 %
Other, total <= 0.50 %<= 0.50 %
Phosphorus, P <= 0.40 %<= 0.40 %
Tin, Sn 11 - 13 %11 - 13 %
Zinc, Zn <= 1.0 %<= 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ampco Metal AMPCOLOY® 712 Tin Bronze, Continuous Cast
Ampco Metal AMPCOLOY® 35 Tin Bronze, Centrifugally Cast
Ampco Metal AMPCOLOY® 35 Tin Bronze, Castings
Ampco Metal AMPCOLOY® 712 Tin Bronze, Centrifugally Cast
Ampco Metal AMPCOLOY® 35 Tin Bronze, Continuous Cast

NAMPCO60 / 15014

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.