MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ THERMOCOMP™ Compound UF009S Polyphthalamide (PPA)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: LNP THERMOCOMP UF009S compound is based on Polyphthalamide (PPA) resin containing 45% glass fiber. Added features of this grade include: Heat Stabilized.

Features: High Stiffness,Heat Stabilized,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.64 g/cc0.0592 lb/in³ISO 1183
 1.645 g/cc0.05943 lb/in³ASTM D792
Moisture Absorption 0.150 %0.150 %Injection Molding
 0.250 %0.250 %23°C/50% RH/24 hrs; ASTM D570
 0.370 %0.370 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0018 cm/cm0.0018 in/in24hrs; ISO 294
 0.0020 cm/cm0.0020 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0046 cm/cm0.0046 in/in24hrs; ISO 294
 0.0050 cm/cm0.0050 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 242 MPa35100 psiASTM D638
 253 MPa36700 psiISO 527
Elongation at Break 1.7 %1.7 %ASTM D638
 1.8 %1.8 %ISO 527
Tensile Modulus 20.35 GPa2952 ksi50 mm/min; ASTM D638
 22.74 GPa3298 ksi1 mm/min; ISO 527
Flexural Strength 386 MPa56000 psiISO 178
 392 MPa56900 psiASTM D790
Flexural Modulus 18.33 GPa2659 ksiISO 178
 18.76 GPa2721 ksiASTM D790
Izod Impact Notched 170 J125 ft-lbASTM D256
Izod Impact, Unnotched 13.45 J/cm25.20 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 14.0 kJ/m²6.66 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 82.0 kJ/m²39.0 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 15.0 J11.1 ft-lbpeak; ASTM D3763
Impact Test 4.00 J2.95 ft-lbMultiaxial Impact; ISO 6603
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 258 °C
@Thickness 3.20 mm
496 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 315 - 325 °C599 - 617 °F
Zone 3 325 - 340 °C617 - 644 °F
Melt Temperature 315 - 330 °C599 - 626 °FInjection Molding
Mold Temperature 140 - 165 °C284 - 329 °F
Drying Temperature 120 - 150 °C248 - 302 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81934 / 289881

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.