MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Dow Dow™ DMDA-8940 HEALTH+™ HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: Dow DMDA-8940 HEALTH+™ HDPE is a narrow molecular weight distribution high density copolymer designed to offer an excellent balance of toughness, environmental stress crack reistance, and processability. This resin is suitable for injection-molded medical devices such as IV kit components and respiratory care. This product can also be used in pharmaceutical packaging including caps and closures.
Main Characteristics:
  • Excellent toughness
  • Excellent stress crack resistance
  • Good processability
  • High gloss parts
Complies with: US FDA 21 CFR 177.1520©3.2a; EU, No 10/2011; Canadian HPFB No Objection; USP XXIII Class VI; Drug Master File Listing. Consult the regulations for complete details.

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: DMF; FDA 21 CFR 177.1520©3.2a; Canadian HPFB No Objection; EU, No 10/2011; USP XXIII Class VI

Form: Pellets

Processing Method: Injection Molding

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.953 g/cc0.0344 lb/in³ASTM D792
Melt Flow 44 g/10 min
@Load 2.16 kg,
Temperature 190 °C
44 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6464ASTM D2240
Tensile Strength at Break 26.9 MPa3900 psiASTM D638
Tensile Strength, Yield 26.9 MPa3900 psiASTM D638
Elongation at Break 10 %10 %ASTM D638
Elongation at Yield 5.0 %5.0 %ASTM D638
Flexural Modulus 1.02 GPa148 ksi2% Secant; ASTM D790B
Tensile Impact Strength 84.0 kJ/m²40.0 ft-lb/in²Type S; ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Melting Point 128 °C262 °F
Crystallization Temperature 116 °C241 °F
Deflection Temperature at 0.46 MPa (66 psi) 71.1 °C160 °FUnannealed; ASTM D648
Vicat Softening Point 123 °C253 °FASTM D1525
Brittleness Temperature -72.2 °C-98.0 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF452 / 311145

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.