MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics G-2 Ceramic Core Material Silica
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: General core type with an intermediate particle size distribution for Equiax castings.

Information provided by Morgan Advanced Materials

Key Words: G-2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.90 g/cc0.0686 lb/in³
Density 2.60 g/cc0.0939 lb/in³
Water Absorption >= 15 %>= 15 %
Open Porosity 28 %28 %
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.0121 GPa1.75 ksi4 point
 
Thermal PropertiesMetricEnglishComments
CTE, linear 1.30 µm/m-°C
@Temperature 25.0 - 1000 °C
0.722 µin/in-°F
@Temperature 77.0 - 1830 °F
Shrinkage 0.60 %0.60 %length, mold-to-fired
 0.80 %0.80 %chord, mold to fired
 
Component Elements PropertiesMetricEnglishComments
Antimony, Sb >= 0.0025 %>= 0.0025 %trace element, 25 ppm
Bismuth, Bi >= 0.00010 %>= 0.00010 %trace element, 1 ppm
Iron, Fe >= 0.090 %>= 0.090 %trace element, 900 ppm
Lead, Pb >= 0.0025 %>= 0.0025 %trace element, 25 ppm
Other 30 %30 %ZrSiO4
Silver, Ag >= 0.0025 %>= 0.0025 %trace element, 25 ppm
SiO2 70 %70 %
Tin, Sn >= 0.0025 %>= 0.0025 %trace element, 25 ppm
Zinc, Zn >= 0.0050 %>= 0.0050 %trace element, 50 ppm
 
Descriptive Properties
Cristobalite Content1 percent, after fire
 5 percent after 15 min at 1390°C
Leachability100 percent, 30 percent boiling KOH, 30 g sample, 30 minutes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF5092 / 200329

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.