MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 2299 X 57352 A Polyetheretherketone (PEEK), Carbon Fiber - PTFE Lubricated - Graphite Powder Lubricated  (discontinued **)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes:

Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.44 g/cc1.44 g/ccASTM D 792
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
@Thickness 3.17 mm
0.0010 - 0.0030 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 155 MPa22500 psiASTM D 638
Elongation at Break 2.0 - 3.0 %2.0 - 3.0 %ASTM D 638
Tensile Modulus 13.8 GPa2000 ksiASTM D 638
Flexural Strength 234 MPa34000 psiASTM D 790
Flexural Modulus 11.0 GPa1600 ksiASTM D 790
Izod Impact, Notched 1.07 J/cm
@Thickness 3.17 mm
2.00 ft-lb/in
@Thickness 0.125 in
D 256
Izod Impact, Unnotched 5.61 J/cm
@Thickness 3.17 mm
10.5 ft-lb/in
@Thickness 0.125 in
ASTM D4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10000 ohm-cm - 1e+0510000 ohm-cm - 1e+05ASTM D 257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 288 °C>= 550 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 349 - 399 °C660 - 750 °F
Mold Temperature 163 - 218 °C325 - 425 °F
Drying Temperature 149 °C300 °F
Dry Time 3 hour3 hour
Moisture Content 0.10 %0.10 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 82.7 - 124 MPa12000 - 18000 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger Tecapeek® XP-101 Compression Molded PEEK Compound, Filled with 15% Graphite and 10% PTFE
Akro-Plastic Akrotek® PEEK CF 40 black (5099) PEEK, Conditioned, 30% Carbon Filled
Ensinger Tecapeek® XP-113 Compression Molded PEEK Compound, 10% PTFE, 15% Graphite, and 3% Carbon Fiber
RTP Company RTP 2203 LF TFE 20  Polyetheretherketone (PEEK) Glass Fiber 20% - PTFE 20% - Low Flow
RTP Company RTP 2285 TFE 15  Polyetheretherketone (PEEK) Carbon Fiber 30% - PTFE 15%

PQZWA634 / 92115

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.