MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT Group QSil 6101 Condensation Cure, Silicone Potting Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QSil 6101 is a 100% silicone solids elastomer designed for electrical potting applications. The two-component system offers quick curing, a low modulus, and is a self-bonding material. This material also has good primerless adhesion to a variety of substrates.

Key Features:

  • 100% solids
  • Fast curing
  • Low viscosity, very flowable
  • Excellent adhesion to many substrates including polycarbonate, PPO/PS & PPE/PS blends
  • UL Listed file number - E205830
  • Meets UL requirements for solar J-box potting

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 g/ccUncatalyzed, Quill Cat 6101
 1.21 g/ccUncatalyzed, QSil 6101
Viscosity 30 cPUncatalyzed, Quill Cat 6101
 6700 cPUncatalyzed, QSil 6101
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30Catalyzed 24 hours @ 25°C
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-1
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Cure Time >= 3.00 hour100% Cohesive Failure; PPO/PS Blends
 >= 6.00 hour100% Cohesive Failure; Aluminum
 >= 16.0 hour100% Cohesive Failure; Polycarbonate
 >= 24.0 hour100% Cohesive Failure; PPE/PS Blends
 24.0 hour
@Temperature 25.0 °C
Catalyzed
Gel Time 4.00 minCatalyzed 24 hours @ 25°C
 
Descriptive Properties
AdhesionCohesive FailureAluminum
 Cohesive FailurePolycarbonate
 Cohesive FailurePPE/PS Blends
 Cohesive FailurePPO/PS Blends
ColorBlackUncatalyzed, QSil 6101
 ClearUncatalyzed, Quill Cat 6101
Lap Shear60 lbfCatalyzed 24 hours @ 25°C, 1000H @ 85°C/85RH
 62 lbfCatalyzed 24 hours @ 25°C, 168H @ 85°C/85%RH
 62 lbfCatalyzed 24 hours @ 25°C, 12H@ RT
 65 lbfCatalyzed 24 hours @ 25°C, 24H@RT
 71 lbfCatalyzed 24 hours @ 25°C, 72H@ RT

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite
Overview of materials for PVC, Rigid Grade
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Aluminum, Al

PACC2106 / 199494

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.