MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Syensqo (Solvay Specialty Polymers) Hyflon® PFA F1520 Perfluoropolymer
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: Hyflon® F is a unique new family of PFA polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low surface energy and exceptional dielectric properties.

Hyflon® PFA F1520 is a low melt flow rate multi purpose resin with an exceptional stress crack resistance, continuous service temperature up to 225°C and a 100-150x10³ cycles flex-life (on a 0.3mm film, ASTM D2176).

Hyflon® PFA F 1520 is an ASTM D3307-16 Type X resin.

Applications: General Purpose; Wire & Cable Applications

Features: Flame Retardant; Good Flexibility; High ESCR (Stress Crack Resist.); Low FlowSolvay recommends that only Color Master Batches based in Hyflon PFA be used. Master Batches based on other fluoropolymers can negatively influence the superior processing and electrical performance of the resin. A list of suppliers can be obtained from your Solvay sales representative.

HEALTH SAFETY AND ENVIRONMENT
- Hyflon PFA F1520 is a very inert polymer and it is not harmful if used and handled according to standard processing procedures. If handled inappropriately, it may release harmful toxic chemicals.
- Hyflon PFA F1520 does not contain any RoHS or WEEE substances. Hyflon MFA F1520 is not produced using APFO and contains no APFO.

PACKAGING AND STORAGE
- Hyflon PFA F1520 resin is available in 25 kg (55 lbs.) and 500 kg (1102 lbs.) packaging. Though it has an indefinite shelf life, it is recommended to store it in a clean area, protected by direct sun light and possible contamination.

Extrusion notes: EXTRUSION PROCESSING GUIDELINES
- As with other fluoropolymers, Hyflon MFA is corrosive in the melt. Therefore all parts coming into prolonged contact with the melt should be made with corrosion resistant materials such as Hastelloy®, Inconel®, Monel® or Xaloy®. Chrome or nickel plating is not recommended since they are typically only sufficient for brief processing tests.
- F1520 is suitable for extrusion using techniques normally applied for other thermo-processable plastics, provided that the extruder is equipped with corrosion resistant alloys. Extruders with L/D ratio of 20:1 to 30:1 are recommended. Extruders should be equipped with independently controlled heaters capable of accurate temperature control up to 450°C (840°F). An overview of the temperature, tooling and equipment requirements are in the following tables.
- Many different screw designs can be used. Single-flight screws are recommended while barrier-flights should be avoided. A typical screw design consist of a long feed section (at least 12 flights), followed by a 2 to 6 flight transition and a 5 to 7 flight metering section.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.11 - 2.16 g/cc0.0762 - 0.0780 lb/in³ASTM D792
Melt Flow 1.0 - 4.0 g/10 min
@Load 5.00 kg,
Temperature 372 °C
1.0 - 4.0 g/10 min
@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 55 - 6055 - 60ASTM D2240
Tensile Strength at Break >= 30.0 MPa>= 4350 psi50 mm/min; ASTM D638
Elongation at Break >= 300 %>= 300 %50 mm/min; ASTM D638
Tensile Modulus 0.400 - 0.500 GPa58.0 - 72.5 ksi1.0 mm/min; ASTM D638
Izod Impact, Notched NBNBASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+17 ohm-cm>= 1.00e+17 ohm-cmASTM D257
Surface Resistance >= 1.00e+17 ohm>= 1.00e+17 ohmASTM D257
Dielectric Constant  2.0
@Frequency 50 Hz
2.0
@Frequency 50 Hz
ASTM D150
 2.0
@Frequency 100000 Hz
2.0
@Frequency 100000 Hz
ASTM D150
Dielectric Strength 35.0 - 40.0 kV/mm
@Thickness 1.00 mm
889 - 1020 kV/in
@Thickness 0.0394 in
ASTM D149
Dissipation Factor  <= 0.00050
@Frequency 50 Hz
<= 0.00050
@Frequency 50 Hz
ASTM D150
 <= 0.00050
@Frequency 100000 Hz
<= 0.00050
@Frequency 100000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 16.0 - 24.0 J/g6.88 - 10.3 BTU/lbDSC
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C66.7 - 111 µin/in-°FASTM D696
Specific Heat Capacity 0.900 - 1.10 J/g-°C0.215 - 0.263 BTU/lb-°FASTM C351
Thermal Conductivity 0.200 W/m-K
@Temperature 40.0 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 104 °F
ASTM C177
Melting Point 265 - 275 °C509 - 527 °F
Crystallization Temperature 255 - 265 °C491 - 509 °FPeak; ASTM D3418
Flammability, UL94 V-0V-0
Oxygen Index 95 %95 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Zone 1 240 - 290 °C464 - 554 °FExtrusion
Zone 2 270 - 320 °C518 - 608 °FExtrusion
Zone 3 300 - 360 °C572 - 680 °FExtrusion
Zone 4 320 - 380 °C608 - 716 °FExtrusion
Zone 5 340 - 390 °C644 - 734 °FExtrusion
Adapter Temperature 370 - 400 °C698 - 752 °FExtrusion
Die Temperature 390 - 420 °C734 - 788 °FExtrusion
Melt Temperature 400 °C752 °FExtrusion
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsPellets
ProcessingExtrusion Coating
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4248 / 280048

http://www.madehow.com/Volume-1/Tire.html

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.