MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sichuan Deyang Haton® hGR60 Polyphenylene Sulfide, Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 60% Glass Fiber Filler

Material Notes: Injection molding

Information provided by Sichuan Deyang Chemical Co., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/ccGB/T 1033.1-2008
Water Absorption 0.020 %GB/T 1034-2008
Linear Mold Shrinkage, Flow 0.0010 cm/cmGB/T 15585-1995
Linear Mold Shrinkage, Transverse 0.0032 cm/cmGB/T 15585-1995
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 115GB/T 3398.2-2008
Tensile Strength 172 MPaGB/T 1040.2-2006
Elongation at Break 1.0 %GB/T1040.2-2006
Flexural Strength 262 MPaGB/T 9341-2008
Flexural Modulus 19.6 GPaGB/T 9341-2008
Izod Impact, Notched (ISO) 10.3 kJ/m²GB/T 1843-2008
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.60e+16 ohm-cmGB/T1410-2006
Surface Resistivity per Square 2.00e+15 ohmGB/T1410-2006
Dielectric Constant 4.0GB/T 1409-2006
Dielectric Strength 14.0 kV/mmGB/T1408.1-2006
Dissipation Factor 0.0010GB/T 1409-2006
 
Thermal PropertiesOriginal ValueComments
Melting Point 280 °CGBT/T 19466.3-2004
Deflection Temperature at 1.8 MPa (264 psi) 270 °CGB/T 1634.2-2004
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese FORTRON 1140L0 PPS, 40% Glass Reinforced
Sichuan Deyang Haton® hGR40 Polyphenylene Sulfide, Glass Fiber Reinforced
Sichuan Deyang Haton® hGR20 Polyphenylene Sulfide, Glass Fiber Reinforced
Celanese Fortron® 1140 L4 Polyphenylene Sulfide (PPS), 40% Glass Fiber

PSICHU906 / 156147

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.