MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sandvik 24.13.LNb Welding strip
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 24.13.LNb is a strip electrode used to obtain a E309LNb corrosion resistant overlay weld deposit on carbon, carbon manganese and low alloyed steels using submerged arc welding (SAW) with Sandvik 10SW flux or electroslag welding (ESW) with Sandvik 49S high speed flux. It gives a 347/E347 chemical composition when used in single layer technique. Sandvik 24.13.LNb can also be combined with Sandvik 19.9.LNb for the second layer to obtain a 347/E347 weld deposit. Other combinations and conditions are possible.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.020 %<= 0.020 %
Chromium, Cr 24 %24 %
Copper, Cu <= 0.30 %<= 0.30 %
Manganese, Mn 2.0 %2.0 %
Molybdenum, Mo <= 0.30 %<= 0.30 %
Nickel, Ni 12.5 %12.5 %
Niobium, Nb (Columbium, Cb) 0.75 %0.75 %
Phosphorus, P <= 0.020 %<= 0.020 %
Silicon, Si 0.30 %0.30 %
Sulfur, S <= 0.020 %<= 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSANDV5125 / 199689

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.