MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mallard Creek Polymers Rovene® 4002 Carboxylated Styrene-Butadiene Emulsion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: ROVENE® 4002 is a medium firm carboxylated styrene - butadiene emulsion designed to have good freeze-thaw stability and low odor characteristics, when used in trade sales coatings. When properly formulated, coatings based on ROVENE® 4002 exhibit tight, continuous films providing the following performance advantages: (1) moisture vapor barrier properties, (2) enamel holdout at higher PVC's than conventional latexes, (3) superior cold temperature coalescence, (4) stability to alkaline substrates and (5) ASTM E-96 perm ratings of 0.5.
APPLICATIONS: ROVENE® 4002 is recommended for use in architectural coatings including flat wall paints and primer-sealers where low perm ratings are needed (1.0 - 0.5 perms).

Information provided by Mallard Creek Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 50 %50 %
Particle Size 0.25 µm0.25 µm
pH 8.58.5
Brookfield Viscosity 600 cP600 cP#2/20 rpm
 
Chemical PropertiesMetricEnglishComments
Styrene Content 65 %65 %
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 4.00 °C39.2 °F
 
Descriptive Properties
EmulsifiersAnionic
Residual Monomer0.01% Max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chosun Refractories CFA-2 Ceramic Foam
Mid-Mountain Materials ARMATEX® SF90 Silicone Rubber Coated Glass Fabric
MetaFoam Metal Foam
Mafic Direct Basalt Roving 10 µm Diameter
LG Chemical Lutex 703 SBR Latex

PMCP041 / 104698

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.