MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

RESPOL REPSOL PRIMEVA® P0720F EVA
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: Product Description: EVA copolymer REPSOL PRIMEVA® P0720F is suitable for injection, blow molding and general extrusion applications when flexibility and toughness are required, even at low temperatures. EVA copolymer REPSOL PRIMEVA® P0720F presents low gel content. It contains antioxidant additives.
Applications: Extrusion; Blow molding; Injection molding. Release agents containing silicone must be avoided.
Recommended melt temperature below 200°C to avoid the decomposition of the polymer. Processing conditions should be optimized for each production line.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: Antioxidant

Features: Antioxidant; Copolymer; Food Contact Acceptable; Low Gel; Low Temperature Flexibility; Low Temperature Toughness

Agency Ratings: EU Food Contact

Processing Method: Blow Molding; Extrusion; Injection Molding

Information provided by REPSOL

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.926 g/cc0.0335 lb/in³ISO 1183
Environmental Stress Crack Resistance >= 100 hour>= 100 hourF50; ASTM D1693
Vinyl Acetate Content 7.5 %7.5 %
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4646ISO 868
Tensile Strength at Break 19.0 MPa2760 psiISO 527-2
Elongation at Break 750 %750 %ISO 527-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 103 °C217 °F
Vicat Softening Point 80.0 °C176 °FISO 306/A
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 °C392 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRESPOL1316 / 312009

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.