System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Wellman Wellamid® GF43-66 XE-N 43% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 40% Glass Fiber Filled
Material Notes:
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.
Data provided by the manufacturer, Wellman Inc.
Key Words:
Polyamide 66
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.49
g/cc
ISO 1183
Water Absorption
1.2 %
Approximate 24 hr.
Linear Mold Shrinkage
0.0020
-
0.0060
cm/cm
ISO 294-4
Mechanical Properties
Original Value
Comments
Tensile Strength, Ultimate
210
MPa
ISO 527
Elongation at Break
3.0 %
ISO 527
Flexural Yield Strength
310
MPa
ISO 178
Flexural Modulus
12.5
GPa
ISO 178
Izod Impact, Notched
1.30
J/cm
ISO 180
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
250
°C
ISO 75
Flammability, UL94
HB
@Thickness 0.790 mm
From Wellman QC Laboratory Testing; UL 94
Processing Properties
Original Value
Comments
Rear Barrel Temperature
540
-
590
°F
Middle Barrel Temperature
530
-
580
°F
Front Barrel Temperature
520
-
570
°F
Nozzle Temperature
520
-
580
°F
Melt Temperature
520
-
580
°F
Mold Temperature
160
-
200
°F
Drying Temperature
175
°F
Opened bags and gaylord boxes
Dry Time
2
-
4
hour
Opened bags and gaylord boxes
Moisture Content
0.050 - 0.20 %
During molding to prevent hydrolytic degradation
<= 0.20 %
In shipping bags, ready to mold
Injection Pressure
5000
-
20000
psi
Back Pressure
50.0
psi
Screw Speed
30
-
120
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Wellman Wellamid® GF13-66 XE-N 13% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized
RTP Company RTP 699 X 94678 SSC-63386 Acrylonitrile Butadiene Styrene (ABS), Phosphorescent Green
RTP Company RTP 199 X 98590 SSC-63791 Polypropylene (PP), Phosphorescent Green
Permabond HM128 Anaerobic Threadlocker
LG Chemical Lupox® TE-5020 High Impact PBT, Thermoplastic Elastomer Alloy, Blow Molding
PWEL18 / 72298
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.