MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
BASF Cetyl Chloroformate
Categories: Fluid

Material Notes: Formula: C17H33ClO2

CAS: 26272-90-2

Description: Cetyl Chloroformate is a colorless to yellowish liquid with a pungent odor. It hydrolyses in the presence of water.

Synonyms: Hexadecyl chloroformate, Palmityloxycarbonyl chloride, Chloroformic acid cetyl ester, Carbonochloridic acid, hexadecyl ester

Applications: Intermediate used in the production of Dyes, Pharmaceuticals, Organic Peroxide compounds and Pesticides

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/cc
Molecular Weight 304.9 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 14.0 °C
Boiling Point 120 °C
Flash Point 120 °C
Ignition Temperature 225 °C
 
Descriptive Properties
Assay>99%Chloroaniline titration
Color<50APHA, DIN EN 1557
CompositionCetyl alcohol<0.5%
 Cetyl chloride<0.3%
 Fe<2 ppm
 HCl<0.01%
 Phosgene<0.01%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Elastollan® 1154 D FHF TPUR Flame Retardant Halogen Free
BASF Elastoblend LP 9192 TPUR
BASF DEHA DI-2-Ethylhexylamine
BASF D 2000 Polyetheramine
BASF Butanediol Divinyl Ether

PBASG0892 / 132525

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.