MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Kaomat SL Blanket
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Thermal Ceramics Kaomat insulation is a non-woven needle-felted "E" fiberglass mat. Kaomat is an economical insulating material used extensively in both the marine and commercial insulation markets. It is noncombustible, chemically stable, resists corrosion and is certifiable to MIL-I-24244 and NRC 1.36.

Features:No “shot” blanket, Excellent dimensional stability, High tensile strength, Available in module form.

Applications:Asbestos replacement, Steam and gas turbine blanket, Insulation of marine exhaust systems, Low temperature (<1200°F {649°C}) insulation, Aluminum homogenizing furnaces, “No-shot” furnace linings.

Information provided by Thermal Ceramics

Data has not been recently verified. Please contact manufacturer for current information.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.144 - 0.160 g/cc0.00520 - 0.00578 lb/in³
Thickness 6300 microns248 mil
 13000 microns512 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 0.0552 - 0.0827 MPa8.00 - 12.0 psi
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0600 W/m-K
@Temperature 260 °C
0.416 BTU-in/hr-ft²-°F
@Temperature 500 °F
 0.0800 W/m-K
@Temperature 371 °C
0.555 BTU-in/hr-ft²-°F
@Temperature 700 °F
 0.110 W/m-K
@Temperature 482 °C
0.763 BTU-in/hr-ft²-°F
@Temperature 900 °F
 0.160 W/m-K
@Temperature 649 °C
1.11 BTU-in/hr-ft²-°F
@Temperature 1200 °F
 0.200 W/m-K
@Temperature 816 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 1500 °F
Melting Point 1700 °C3100 °F
Maximum Service Temperature, Air 871 °C1600 °FContinuous
 982 °C1800 °FRating
Shrinkage  4.0 %
@Temperature 649 °C,
Time 86400 sec
4.0 %
@Temperature 1200 °F,
Time 24.0 hour
Linear
 6.0 %
@Temperature 816 °C,
Time 86400 sec
6.0 %
@Temperature 1500 °F,
Time 24.0 hour
Linear
 
Component Elements PropertiesMetricEnglishComments
SiO2 >= 94 %>= 94 %
 
Descriptive Properties
Fiber Diameter, microns6-13
Fiber Length, cm5-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Thermal Ceramics Kaomat Blanket
Rogers Arlon 920-20Bxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape
Mid-Mountain Materials CERMEX® MT1200 Thermal Insulation Mat

CTHERM007 / 2327

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.