TABOREN-PC 59 C 40 is a compound based on polypropylene copolymer filled with 40% of calcium carbonate filler, stabilized with a UV/AOX package. It is designed for injection molding technology and used in many industrial fields with stress put on excellent processability and good surface performance.Information provided by Silon US LLC. |