MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chemours Teflon® PTFE Grade FPD3584 Aqueous Dispersion  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: DuPont PTFE FPD3584 is a negatively charged, hydrophobic colloid, containing approximately 60% (by total weight) of 0.05 to 0.5 mm polytetrafluoroethylene (PTFE) resin particles suspended in water. Seen as a milky white liquid, it also contains approximately 6% (by weight of PTFE) of a nonionic wetting agent and stabilizer. Viscosity at room temperature is approximately 20 cP. Nominal pH is 10.

DuPont PTFE FPD3584 dispersion is a generalpurpose impregnation grade of dispersion.

When properly processed, the PTFE resin in DuPont PTFE FPD3584 exhibits the superior properties typical of the fluoropolymer resins: retention of properties after service at 260°C (500°F), useful properties at –240°C (–400°F), chemical inertness to nearly all industrial chemicals and solvents, and low friction and antistick surfaces. Dielectric properties are outstanding and stable with frequency and temperature.

Applications

DuPont PTFE FPD3584 is normally used to impregnate packings for sealing and low friction applications. The small particle size, low surface tension and low viscosity aid in wetting of the braided yarn bundles. Typical substrates that can be impregnated include PTFE fibers, aramid, flax, glass, etc.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Key Words: Polytetrafluoroethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc1.50 g/ccASTM D4441
Base Resin Density 0.900 g/cc0.0325 lb/in³Weight of PTFE resin solids; ASTM D4441
Solids Content 60 %60 %Percent of PTFE resin solids; ASTM D4441
Particle Size 0.20 µm0.20 µmAverage dispersion particle size
pH 9.59.5ASTM E70
Viscosity 20 cP
@Temperature 25.0 °C
20 cP
@Temperature 77.0 °F
ASTM D2196
 
Thermal PropertiesMetricEnglishComments
Melting Point 327 °C621 °FASTM D1457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Teflon® PTFE Grade 7B Granular Compression Molding Resin
Chemours Teflon® PTFE Grade 30 Aqueous Dispersion
Chemours Teflon® PTFE CFP6000 Resin for Lubricated Paste Extrusion
Chemours Teflon® PTFE 7A Granular Molding Powder
Chemours Teflon® PTFE 6C Resin for Lubricated Paste Extrusion

PDU9209 / 33328

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.